Rubber & Plastic Products

Natural Pigments Compound Into PLA and PBS, but Light Stability Still Limits Use

Mirela ConstantinNovember 2, 20265 min read6 views

At a glance

  • A study finds four natural colorants survive twin-screw compounding with PLA and PBS with little effect on melt flow or mechanical performance, while UV exposure remains the main obstacle.
  • Masterbatches based on spirulina, curcumin, beetroot and chlorophyllin were compounded into PLA and PBS at 2–6 wt% without major changes to melt viscosity or mechanical behavior, although spirulina could not withstand PLA's 190 °C profile. Most formulations shifted visibly in color after 50 hours of xenon-lamp exposure, leaving lightfastness as the largest barrier to wider adoption.
Four colored polymer strands emerging from a laboratory twin-screw extruder, next to dishes of natural pigment powder and a row of molded color chips, one of which has faded.

Four commercial natural colorants — blue spirulina, yellow curcumin, red beetroot and green chlorophyllin — can be converted into color masterbatches and compounded into polylactic acid (PLA) and polybutylene succinate (PBS) on standard twin-screw extrusion and injection molding equipment, according to a study on natural pigment-based colour masterbatches and their application in biopolymers. Processing behavior and mechanical properties stayed close to those of the uncolored polymers. Photostability did not.

The work examined how each pigment survives melt processing, what it does to melt flow, tensile and impact behavior, and how the resulting compounds hold up under accelerated light exposure.

Masterbatches and a narrowed processing window

The pigments were compounded with PLA and PBS into masterbatches by twin-screw extrusion, then let down into the matching polymer matrix at 2, 4 and 6 wt% and injection molded into test specimens. The formulation also contained titanium dioxide, calcium carbonate and stearic acid, included to support UV protection, pigment dispersion and processing.

Heat is the central constraint. Natural pigments are organic and begin to break down at lower temperatures than the polymers that carry them. Thermogravimetric analysis placed degradation onset at roughly 229 °C for spirulina, 244 °C for curcumin, 258 °C for chlorophyllin and 267 °C for beetroot, below the degradation temperatures recorded for PLA and PBS.

The researchers therefore selected temperature profiles that melted each polymer while limiting thermal exposure of the pigments: 145 °C for PBS and 190 °C for PLA, with the twin-screw extruder running at 65 rpm and a feed rate of 2 kg/h.

Spirulina fails in PLA, survives in PBS

That window suited most pigment–polymer pairs, with one clear exception. Spirulina lost its characteristic blue during PLA processing, so a blue PLA masterbatch could not be produced. PBS, processed at 145 °C, preserved enough pigment stability for successful compounding. The outcome indicates that pigment compatibility depends strongly on the thermal processing requirements of the matrix, not on the colorant alone.

Melt flow and mechanical properties barely move

Rheologically, the pigments caused only limited change. Melt flow rate decreased slightly after incorporation, indicating a modest rise in melt viscosity. Neat PLA measured about 50 g/10 min, and the natural-pigment masterbatches stayed near that value; PBS responded similarly with a minor reduction.

That matters to compounders, because a natural color system offers little practical value if it forces substantial changes to screw design, pressure settings or molding conditions. Here, conventional twin-screw compounding and injection molding handled most formulations without major difficulty.

Tensile and impact behavior were also largely preserved across the 2 to 6 wt% range. PLA started at a Young's modulus of about 1710 MPa and a tensile strength of 65.6 MPa; PBS started at about 392 MPa and 34.5 MPa. Colored formulations stayed close to those baselines, and impact strength remained in a similar range, although individual pigments introduced some variation.

Color fastness is the open problem

Successful extrusion did not translate into durable color. After 50 hours of xenon-lamp exposure, most formulations exceeded a color difference of ΔE* = 2, the level at which a change becomes visually perceptible. The PLA formulation containing 2 wt% green chlorophyllin masterbatch was the main exception and showed the highest photostability.

The study points to UV stability as the largest barrier to broader use. Packaging, consumer products, agricultural parts and outdoor applications would likely require additional stabilization, protective coatings or pigment modification before natural colors can compete with conventional systems over long service periods.

Lower carbon footprint, unfinished performance

The environmental comparison favored the natural route under the study's assumptions: one kilogram of curcumin pigment corresponded to about 0.04 kg CO2-eq, against 18.65 kg CO2-eq for the inorganic green reference pigment. The natural-pigment masterbatches also consumed less electricity during extrusion and pelletizing.

The study concludes that further development is needed on lightfastness and thermal stability, but that several natural colorants can already be compounded into PLA and PBS on conventional equipment with only limited shifts in melt viscosity and mechanical performance.

Reported by Mirela Constantin, Industrial Seals and Hoses Analyst.